1. In the polishing process, using wet grinding drum rinse toner method is simple and rapid, economic, stable quality.
2. Rinsing toner is a kind of synthetic abrasive hardness, its thickness is suitable, will not scratch the surface, especially suitable for wet grinding and washing barrel color. Wide use.
1.Operating conditions:
The first process: rough mill
The work piece 60 ~ 80kg, time 5 ~ 20 minutes, several ingredients, brushing powder is 0.5 ~ 2kg, the water added to the barrel full of 60%
Second pass process: fine polishing
The work piece 60 ~ 80kg, time 10 ~ 30 minutes, some ingredients, tea seed powder is 0.8 ~ 2 kg, the water added to about 60% , neutral oil removal agent 50 ~ 100ml.
2.Product catalog: Brushing powder, tea seed powder, neutral degreasing agent.