B-3 electrolytic oil removing agent containing electrolytic builder. Applicable to iron and steel in addition to oil, the ability of removing oil if fast, low foam, not hanging ash, water washing, easy to use, and durable.
1.Makeup method:
First, add water to the tank 3/4 volume, heating up to 50-60 ℃ Celsius, according to the volume of electrolysis oil removing agent join the B-3, stirring to fully dissolve, add water to the working surface, heating to the temperature process, can be produced.
2.Operating conditions:
The appearance of color mortar or slightly yellow, powder. Agglomeration does not affect product quality. The pH ≥13 is not easy to contact with acid. The ratio of tank concentration B-3 and water is 3 ~ 10%, oil removing temperature is 15-70℃, the best temperature is 60 ℃, removing oil time ultrasonic, barrel light 2 ~ 5 minutes, soak 5 ~ 30 minutes.
3.Product catalog: Electrolytic removing agent